Eritishni oson olib tashlash uchun past erish nuqtasi lehim qotishmasini tayyorlang.
Iltimos, mening blogimga tashrif buyuring.
Materiallar
Vismut metall 2,5 g
63/37 Rosin yadroli lehim 2,5 g
1 -qadam:
Ularni Yapon Sake kubogiga soling.
Gaz brülörü bilan isitish.
Iltimos, mening blogimga tashrif buyuring.
2 -qadam:
Sake kubogida lehimli temir bilan eritib cho'zing.
Iltimos, mening blogimga tashrif buyuring.
3 -qadam:
KO'RING 1
Qotishma bilan Arduino Nano -dagi Desolder IC.
Iltimos, mening blogimga tashrif buyuring.
4 -qadam:
KO'RING 2
Qotishma bilan Arduino Nano -da Desolder 328P.
Iltimos, mening blogimga tashrif buyuring.
5 -qadam:
Erish uchun issiqlik va qotishma termojuft bilan harorat o'zgarishini tekshirish.
Qotishma erish nuqtasi 97 daraja. C (207 daraja F).